Polyolefin Shrink Film - HS
|
| Gauge | ![]() |
![]() |
45 | 60 | 75 | 100 |
![]() |
Unit | Test Method |
![]() |
![]() |
![]() |
![]() |
| Yield | Sq. in. per pound | ![]() |
66,000 | 50,000 | 40,000 | 30,000 |
| Tensile properties: | ![]() |
![]() |
MD TD | MD TD | MD TD | MD TD |
| Modulus of elasticity | N/mm² | D-882A | 320 360 | 310 350 | 300 380 | 290 340 |
| Tensile strength | N/mm² | D-882 | 100 100 | 100 100 | 100 100 | 100 100 |
| Elongation | % | D-882 | 100 100 | 120 120 | 130 130 | 165 165 |
| Seal Strength | gr/cm gr/cm² |
Int. meth. | 855 | 1025 | 1300 | 1655 |
| Tear propagation | gr | D-1922 | 6.5 | 8.5 | 10.5 | 13.5 |
| Cof. film-film, kinetic | adim. | D-1894 | 0.30 | 0.40 | 0.40 | 0.50 |
| Shrink at 250°F | % | ![]() |
MD TD 68 68 |
MD TD 60 65 |
MD TD 60 65 |
MD TD 60 65 |
| Gas permeablility: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| WVTR | gr/m²24h | E-96 | 18 | 16 | 12.5 | 10 |
| O² permeability | gr/m²24h/am | D-3985 | 18000 | 12000 | 10000 | 8000 |
| CO² transmission | gr/m²24h/am | D-1434 | 20000 | 19800 | 17000 | 16000 |
| Optical properties: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| Haze | % | D-1003 | 1.5 | 1.8 | 2.2 | 2.4 |
| Gloss | photoc. | D-2457 | 145 | 145 | 145 | 130 |