![]() ADVANCED TECHNOLOGY IN PLASTIC MATERIALS |
Omnia USA |
Home | PRODUCTS | Become a Distributor | About Our Products | Contact Us |
|
|
|
Polyolefin Shrink Film - HS
|
|
| Gauge | ![]() |
![]() |
45 | 60 | 75 | 100 |
![]() |
Unit | Test Method |
![]() |
![]() |
![]() |
![]() |
| Yield | Sq. in. per pound | ![]() |
66,000 | 50,000 | 40,000 | 30,000 |
| Tensile properties: | ![]() |
![]() |
MD TD | MD TD | MD TD | MD TD |
| Modulus of elasticity | N/mm² | D-882A | 320 360 | 310 350 | 300 380 | 290 340 |
| Tensile strength | N/mm² | D-882 | 100 100 | 100 100 | 100 100 | 100 100 |
| Elongation | % | D-882 | 100 100 | 120 120 | 130 130 | 165 165 |
| Seal Strength | gr/cm gr/cm² |
Int. meth. | 855 | 1025 | 1300 | 1655 |
| Tear propagation | gr | D-1922 | 6.5 | 8.5 | 10.5 | 13.5 |
| Cof. film-film, kinetic | adim. | D-1894 | 0.30 | 0.40 | 0.40 | 0.50 |
| Shrink at 250°F | % | ![]() |
MD TD 68 68 |
MD TD 60 65 |
MD TD 60 65 |
MD TD 60 65 |
| Gas permeablility: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| WVTR | gr/m²24h | E-96 | 18 | 16 | 12.5 | 10 |
| O² permeability | gr/m²24h/am | D-3985 | 18000 | 12000 | 10000 | 8000 |
| CO² transmission | gr/m²24h/am | D-1434 | 20000 | 19800 | 17000 | 16000 |
| Optical properties: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| Haze | % | D-1003 | 1.5 | 1.8 | 2.2 | 2.4 |
| Gloss | photoc. | D-2457 | 145 | 145 | 145 | 130 |
These are typical values for Omnia shrink film. They are not intended for use as limiting specifications. Omnia shall have no liability whatever for the results obtained through use of this data. Dry storage below 90°F is recommended. Prolonged exposure to temperature above 90°F may cause difficulty in unwinding film. |
| Gauge | ![]() |
45 | 60 | 75 | 100 |
| Rolls Lengths | ![]() |
![]() |
![]() |
![]() |
![]() |
| Flat film | Ft | 10,500 | 8,750 | 7,000 | 5,250 |
| Folded film | Ft | 5,250 | 4,375 | 3,500 | 2,626 |
| Rolls width: | ![]() |
![]() |
![]() |
![]() |
![]() |
| Flat film | In | from 4 to 90 | |||
| Folded film | In | from 4 to 90 | |||
| Inner diameter | In | 3 | |||
| Outer diameter | In | 9.5 | |||
Cross-Linked Shrink Film - CX
|
| Gauge | ![]() |
![]() |
45 | 60 | 75 | 100 |
![]() |
Unit | Test Method |
![]() |
![]() |
![]() |
![]() |
| Yield | Sq. in. per pound | ![]() |
66,000 | 50,000 | 40,000 | 30,000 |
| Tensile properties: | ![]() |
![]() |
MD TD | MD TD | MD TD | MD TD |
| Tensile strength | N/mm² | D-883 | 125 115 | 120 100 | 125 105 | 110 100 |
| Elongation | % | D-884 | 105 100 | 105 100 | 110 107 | 120 115 |
| Seal Strength | N/mm² | Int. meth. | 71 | 67 | 65 | 60 |
| Tear propagation | gr | D-1922 | 7.3 | 10 | 11.5 | 13 |
| Cof. film-film, kinetic | adim. | D-1894 | 0.26 | 0.25 | 0.25 | 0.25 |
| Shrink at 250°F | % | D-2732 | MD TD 70 71 |
MD TD 68 69 |
MD TD 67 67 |
MD TD 66 66 |
| Optical properties: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| Haze | % | D-1003 | 1.5 | 1.7 | 2 | 2.4 |
| Gloss | photoc. | D-2457 | 131 | 125 | 123 | 121 |
Anti-Fog Cross-Linked Shrink Film - AF
|
| Gauge | ![]() |
![]() |
45 | 60 | 75 | 100 |
![]() |
Unit | Test Method |
![]() |
![]() |
![]() |
![]() |
| Yield | Sq. in. per pound | ![]() |
66,000 | 50,000 | 40,000 | 30,000 |
| Tensile properties: | ![]() |
![]() |
MD TD | MD TD | MD TD | MD TD |
| Tensile strength | N/mm² | D-883 | 125 115 | 120 100 | 125 105 | 110 100 |
| Elongation | % | D-884 | 105 100 | 105 100 | 110 108 | 120 115 |
| Seal Strength | N/mm² | Int. meth. | 71 | 67 | 65 | 60 |
| Tear propagation | gr | D-1922 | 7.3 | 10 | 11.5 | 13 |
| Cof. film-film, kinetic | adim. | D-1894 | 0.26 | 0.26 | 0.25 | 0.25 |
| Shrink at 250°F | % | D-2732 | MD TD 70 71 |
MD TD 68 69 |
MD TD 67 67 |
MD TD 66 66 |
| Optical properties: | ![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
| Haze | % | D-1003 | 1.6 | 2 | 2.1 | 2.4 |
| Gloss | photoc. | D-2457 | 125 | 120 | 123 | 121 |
PVC Shrink Film
|
|
|
| PROPERTIES | UNITS | VALUES | TEST | |||
| TYPE | ![]() |
SHR 15 | SHR 19 | ![]() |
||
| Thikness | Gauge | 60 | 75 | ASTMD 374 | ||
| Density | Kg/dm³ | 1.3 | ![]() |
|||
| Weight | g/m² | 19.5 | 24.7 | ASTMD 1505 | ||
| Yield | m²/Kg | 51.28 | 40.48 | ASTMD 646 | ||
![]() |
![]() |
L | T | L | T | ![]() |
| Tensile Strength | Kg/cm² | 810 | 590 | 850 | 630 | ASTMD 882 |
| Elongation | % | 85 | 110 | 91 | 118 | ASTMD 882 |
| Internal Tear Strength | g | 6 | 6 | 6 | 6 | ASTMD 1922 |
| Limit of elasticity | Kg/cm² | 5800 | 5200 | 5700 | 5300 | ASTMD 882 |
| Shrinkage at 190°F | % | 42 | 37 | 40 | 38 | PPTM |
| Shrinkage Stress | Kg/cm² | 13.7 | 10.1 | 14 | 10.8 | ASTMD 1504 |
| Sealing Strength | g/cm | 550 | 680 | PPTM | ||
| Sealing Temperature | °F | 250 / 320 | PPTM | |||
| Impact Strength | cm/Kg | 7 | 10 | ASTMD 3420 | ||
| Gas Permeability | ![]() |
![]() |
![]() |
|||
| O² | 24h/ | 820 | ![]() |
|||
| Nitrogen | m²/ | 190 | ASTMD 1434 | |||
| CO² | 1 atm/ | 3950 | ![]() |
|||
| W.U.T.R. | G/24h/m² | 110 | 88 | E96 | ||
| Slip Coefficient | ![]() |
Less than 1 | ASTMD 7894 | |||